Split Tube Furnace with 60mm Ni-Based Superalloy Tube for 10E-6 Torr High Vacuum and 300 PSI High Pressure

Split Tube Furnace with 60mm Ni-Based Superalloy Tube for 10E-6 Torr High Vacuum and 300 PSI High Pressure
Product Detailed
The furnace also can be used under high pressure upto 20 atm both in oxygen and inert gas. Product Description

OTF1200X-60UV is CE certified 60mm dia. Ni based super-alloy tube furnace with CF flange and KF25 adaptor for ultra- high vacuum application upto  10^-6 torr and 1200°C. Precision temperature controller can provide 30 segments programmable profile with +/- 1°C accuracy.   The furnace also can be used under high pressure upto 20 atm both in oxygen and inert gas.

Specifications:

Furnace casingDouble layer steel casing with air cooling to keep furnace surface temperature lower than 60°C.High purity fibrous alumina insulation for Max. energy saving.
Power

3.0  KW  Max. ( 20A breaker required)

VoltageAC 208-240 Single Phase, 50/60 Hz
Max. Temperature1100°C  ( < 1 hour )
Continuous Temperature1000°C
Max. Heating Rate <= 30°C /min
Processing TubeMaterial: Nickel based super-alloy seamless tube with max. 1200°C working temperature  Tube Size:  OD 60 x  ID 52 x  Length 1000 (mm) 
Heating Zone length440 mm ( single zone )
Constant temperature zone150  mm (+/-1°C)
Temperature controllerPID automatic control with 30 steps programmable Automatic ver-temperature and thermal broken protection
Temperature Accuracy+/ - 1°C

Vacuum Sealing & Connection

Two sets of CF-63 flanges are included in the standard package:High Vacuum CF-63 Flange: KF40 vacuum pump connector, KF25 vacuum pressure senser connector, right-angle vacuum valves and one meter long SS bellows are installed in one side flange for connecting to vacuum pump.  (for use under high pressure only )High Pressure CF-63 Flange: 1/4" swagelok connector and SS needle valve are installed in another flange for gas flow. (for use under high pressure) 
Pressure limited

 Under High Pressure:   Warning:  Must limit working temperature under a certain positive pressure limited by vessel material strength

800 PSI max      at  800°C  (50 bar)300 PSI max.     at 1000°C (20 bar)130 PSI max.     at 1100°C (9 bar )Never heat up vessel above 1200oCUnder high vacuum1E-2 torr by a mechanical pump5E-6 torr by a compact molecular pumpPlease order vacuump pump by click picture below at extra cost

.

Heating Element

 Fe-Cr-Al Alloy doped by Mo